Si-TPV 3100-55A ba wai kawai kayan masarufi ne masu amfani ba, har ma yana da ingantaccen gyare-gyare da ƙari wanda aka yi da silicone. Wannan haɗin yana ba da taɓawa mai laushi mai ɗorewa, mai sauƙin shafawa da kuma juriya ga tabo. Ba ya ɗauke da robobi da masu laushi, yana tabbatar da aminci da aiki ba tare da wani ruwan sama ba, koda bayan an yi amfani da shi na dogon lokaci. Wannan jerin yana aiki azaman ingantaccen ƙari na filastik da mai gyara polymer, wanda hakan ya sa ya dace da haɓaka tsarin thermoplastic polyurethane (TPU) ko thermoplastic elastomer (TPE).
Si-TPV ba wai kawai yana ba da jin daɗi da laushi ba, har ma yana rage taurin TPU, yana cimma daidaiton kwanciyar hankali da aiki mai kyau. Yana ba da ƙarewa mai laushi, tare da juriya da gogewa, wanda hakan ya sa ya zama mafita mafi kyau ga aikace-aikace daban-daban, gami da kayan masarufi, sassan motoci, kebul na caji na EV, na'urorin likitanci, bututun ruwa, bututun ruwa, da kayan wasanni - inda jin daɗi, dorewa, da kyawun gani suke da mahimmanci.
Ba kamar sauran abubuwan da aka ƙara a silicone na gargajiya ba, ana samar da Si-TPV a cikin nau'in pellet kuma ana sarrafa shi kamar thermoplastic. Yana warwatsewa sosai kuma daidai gwargwado a cikin matrix na polymer, tare da ɗaure copolymer a zahiri, yana hana ƙaura ko "fure." Wannan ya sa Si-TPV ya zama mafita mai aminci da ƙirƙira don cimma saman laushi mai laushi a cikin elastomers na thermoplastic ko wasu polymers, ba tare da buƙatar ƙarin sarrafawa ko rufewa ba.
| Ƙarawa a Hutu | 571% | ISO 37 |
| Ƙarfin Taurin Kai | 4.56 Mpa | ISO 37 |
| Bakin Teku A Taurin | 53 | ISO 48-4 |
| Yawan yawa | 1.19g/cm3 | ISO1183 |
| Ƙarfin Yagewa | 41kN/m | ISO 34-1 |
| Modulus na Ragewa | 1.79Mpa | |
| MI(190℃,10KG) | 58 | |
| Zafin Narkewa Mafi Kyau | 165 ℃ | |
| Mafi kyawun Zafin Mold | 25 ℃ | |
1. Yin allura kai tsaye.
2. A haɗa SILIKE Si-TPV 3100-55A da TPU a wani rabo, sannan a fitar da su ko a yi musu allura.
3. Ana iya sarrafa shi dangane da yanayin sarrafa TPU, ana ba da shawarar zafin aiki shine 160 ~ 170 ℃.
1. Ana iya ƙera samfuran Si-TPV elastomer ta amfani da hanyoyin kera thermoplastic na yau da kullun, gami da yin molding fiye da kima ko yin molding tare da substrates na filastik kamar PP, PA.
2. Jin siliki sosai na Si-TPV elastomer baya buƙatar ƙarin matakai na sarrafawa ko rufewa.
3. Yanayin aikin na iya bambanta dangane da kayan aiki da hanyoyin aiki daban-daban.
4. Ana ba da shawarar busar da danshi mai bushewa da bushewa ga duk busarwa.
25KG / jaka, jakar takarda mai sana'a tare da jakar ciki ta PE.
A kai shi a matsayin sinadari mara haɗari. A adana a wuri mai sanyi da iska mai kyau.
Halayen asali za su kasance ba tare da matsala ba na tsawon watanni 12 daga ranar samarwa idan aka ajiye su a cikin ajiyar da aka ba da shawarar.